CHIMEI ABS PA-747 vs PA-709: Properties & Differences

Side-by-side comparison of two genuine POLYLAC ABS grades to help you select the right one.

PA-747

High-impact ABS for tough, drop-resistant components.

Full specs »

PA-709

Super-high-impact, low-temperature ABS for cold-environment parts.

Full specs »

Property comparison

PropertyPA-747PA-709
Melt Flow Rate16 g/10min20 g/10min
Density1.04 g/cm³1.03 g/cm³
Tensile Strength42 MPa40 MPa
Izod Impact35 kJ/m²55 kJ/m²
Heat Deflection Temp90 °C90 °C
FlammabilityHB -HB -

PA-747 is better when

Choose PA-747 when toughness beats gloss. For even colder environments or extreme impact, move to PA-709; for extruded sheet/pipe, use PA-747S.

PA-709 is better when

Pick PA-709 when the part lives in cold or takes severe impact; it is the low-temp king of the high-impact family. For extrusion use PA-709P.

Which should I choose, PA-747 or PA-709?

PA-747 vs PA-709: PA-709 is the super-high-impact/low-temp grade; PA-747 covers general high-impact needs at lower cost. PA-709 vs PA-747: PA-709 for low-temp/severe impact; PA-747 for general high-impact at lower cost.

Can I get both grades in one shipment?

Yes - mixed containers are available. Contact us on WhatsApp for a combined quotation.